Although shiny joints are not an IPC/J-STD requirement, you can minimize dullness by using nitrogen in your oven, or, by changing solder pastes. Some pastes provide for shinier joints than others. But again, shininess is not a requirement.
-Carrie
-----Original Message-----
From: Poh Kong Hui [mailto:[log in to unmask]]
Sent: Thursday, February 27, 2003 7:18 AM
To: [log in to unmask]
Subject: [TN] : Shining smooth solder joint on ENIG or Gold plating
Board.
Importance: High
Hi Technetters,
Can someone advise me how to get a good smooth shining solder joint on the
ENIG board or board with gold plate SMT pads.
As I can understand that board subjected to reflow soldering, the solder
joint tends to look dull and not so smooth joint. But, is there any way to
get a good shining joint.
Thanks.
Poh
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|