TECHNET Archives

February 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Content-Type:
text/plain; charset="ISO-8859-1"
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>
Date:
Wed, 26 Feb 2003 09:10:00 -0800
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Rick Thompson <[log in to unmask]>
Subject:
From:
Rick Thompson <[log in to unmask]>
Content-Transfer-Encoding:
7bit
Sender:
Parts/Attachments:
text/plain (78 lines)
Daan,

While the DRS24 is a nice system, I think it may have some of the same
limitations as other hot-air machines of it's vintage. Airflow on these
machines tends to move small parts around.  If you switch to a low flow
option, it's sometimes difficult to get enough heat, especially if you have
a small footprint board. We have both SRT 1100 and a DRS24 and find similar
limitations.  It does also need nozzles.  A couple of systems I've looked at
recently were impressive with their ability to handle small components.
Metcal has a couple of hot-air units that are designed to handle very small
BGAs, micro-BGAs, CSPs, etc. ERSA has an IR unit that we were very impressed
with. It handled boards from small PCMCIA size to large 8x12 boards that are
bonded to a .400" aluminum heatsink on both sides. It depends on visually
watching the BGA ball drop, so it has some limitations due to visibility,
but overall for a wide variety of work, it would be one I looked at.

Rick Thompson

Sr. SMT Process Engineer
SMTEK International, Inc.
+1 (805) 532-2800
[log in to unmask]


===== Original Message from [log in to unmask] (TechNet E-Mail Forum.) at
2/26/03 8:30 am
>Hi Technet,
>
>We're planning to replace our current BGA repair equipment by something
>that's more suitable for fine-pitch BGA's and microBGA's (ballpitches
>down to 0.5 mm).
>We can get a brandnew Airvac DRS24 (or Zevac, as it's called in Europe)
>for half the price, but then we need to decide about it very soon,
>without having the time to do a good evaluation.
>Time to seek some expert's advice.....
>
>A significant part of our production work is subcontracting, and new
>customer-relations often start with doing some BGA-repairs for them.
>It's always urgent (no time to order a nozzle), there's never a sample
>board to adjust the profile, and normally there's hardly any free area
>around the BGA. We see everything from fine-pitch BGA's to CBGA's, 40*40
>mm heatsinked-BGA's and BGA-sockets, on boardthicknesses up to 5 mm.
>From what I heard the Airvac is certainly one of the very best
>rework-machines on the market, but I'm not sure if it is the best choice
>(i.e. flexible enough) for our situation.
>
>Any recommendations ?
>
>Daan Terstegge
>Thales Communications
>Unclassified mail
>Personal Website: http://www.smtinfo.net
>
>---------------------------------------------------
>Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
>information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
>ext.5315
>-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2