Hey Eddie,
I've never heard of anyone wanting lamination (resin) voids intentionally,
ha ha. You might tinker with a sequential lam and a forming release sheets
(oh, what's that stuff called? - racking Diet Coke soaked brain).
The alternative of mechanically removing the unneeded layers but I wouldn't
a high volume job.
As a demo sample we laminated a board half with prepreg and the other half
without. The copper tarnished but it was a great visual aid. Something
similar might work for ya.
H
~~~~~~~~~~~~~~~~~~~~~~~~~~~
Hans M. Hinners
AC-130 Systems Engineer (Hardware)
Warner Robins Air Logistics Center (WR-ALC)
226 Cochran Street
Robins AFB, GA 31098-1622
Tele: (478) 926 - 5847 [DSN Prefix: 468]
Fax: (478) 926 - 4911
mailto:[log in to unmask]
-----Original Message-----
From: Eddie Rocha [mailto:[log in to unmask]]
Sent: Friday, February 21, 2003 2:19 PM
To: [log in to unmask]
Subject: [TN] Multilyayer w/ open cavities
Any advise on the best approach on how to build a multilayer PCB
with open cavities exposing an internal layer?
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|