Lorraine, Depending on quantities involved, it may be cost effective
to have the spec call out a slightly larger dimension(to keep from going
undersize, and then pay someone to trim or sand the boards down to within
your final spec. Just my two cents worth! Good luck, Dave Dixon,
Aero-Mach Labs Inc.
On Tue, 18 Feb 2003 16:58:04 -0000, Reid, Lorraine
<[log in to unmask]> wrote:
>Can anyone please advise if it is possible to rout a bare PCB (fab) to a
>tolerance of +/- 0.05 mm? The board is 0.8mm thick.
>
>One of our vendors is telling us that they can't manufacture to this and
>that they don't believe it is possible. A second vendor has led us to
>believe that they can do but experience tells us that they aren't making
>it! For info the boards are designed to fit snugly into a plastic
>housing with no other means of fixing - hence the tight tolerance.
>
>Thanks in advance for any feedback received.
>
>Lorraine Reid
>
>
>---------------------------------------------------
>Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
>information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
>-----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|