As the industry moves toward tin coatings for component leads, concern about tin whiskers for large, long design life systems has increased. NEMI has a project working to understand the basic mechanism for whisker formation. NEMI, NIST and TMS are co-sponsoring a workshop in conjunction with the TMS annual conference in San Diego on Sunday, March 1 at the San Diego convention center. This will be a specialist workshop sharing the latest research and theories on tin whisker formation. Details of the workshop including a sign-up form are available at www.nemi.org. There is no fee to attend.
Ron Gedney
NEMI Consultant
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|