Hi Per-Erik,
Thanks for the info. Is it possible for you to send me a copy of P.L. Tu et
al. "Effect of Intermetallic Compounds on Vibration Fatigue of µBGA Solder
Joints," IEEE Trans. on Advanced Pack., Vol. 24, No.2, 2001? Unfortunately, I
do not have acces to IEEE Trans.
>the crack formation moved from the board side (Ni/solder interface) to the
component side (Cu/solder interface) < would imply interfacial separation not
cracks in the IMC?
>CU-IMC/solder interface or between Cu6Sn5 and Cu3Sn IMC layers<, both of
these are interfacial, but "between Cu6Sn5 and Cu3Sn IMC layers" is
definitely a new one for me--sure cannot think of a good mechanism.
One possibility is impurities accummulting at these interfaces given the long
exposure to 120C; this would also explain the move from the board side
(Ni/solder interface) to the component side (Cu/solder interface).
Regards,
Werner Engelmaier
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|