TECHNET Archives

February 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Carlr Ray <[log in to unmask]>
Date:
Tue, 18 Feb 2003 07:39:57 +0100
Reply-To:
Subject:
From:
Jowan Iven <[log in to unmask]>
Content-Type:
text/plain; charset="iso-8859-1"
In-Reply-To:
Content-Transfer-Encoding:
7bit
MIME-Version:
1.0
Parts/Attachments:
text/plain (85 lines)
Hello Carl,

It's hard to give advise without seeing the design.
But, like Kathy, I strongly recommend another board finish.
Never seen a HASL that was flat enough for 16 mil pitch.
ENIG is what we use for fine-pitch applications.

Hope this helps a little.


Jowan Iven


-----Original Message-----
From:   TechNet [mailto:[log in to unmask]] On Behalf Of Carlr Ray
Sent:   maandag 17 februari 2003 23:26
To:     [log in to unmask]
Subject:        [TN] 16mil QFP Process Issues

Hey Techneters,
I have a couple of questions you guys maybe able to help with (at least
I want some advice). The questions below pertain to some assembles I
will be developing some processes for in the near future. These units
have the following technology: 16 mil QFP, uBGA .65 mil and 1 mil pitch,
multiple PBGA 300+ ball count, PTH components (radial and axial types),
double sided, HASL  surface finish.

1. For 16 mil QFPs and uBGAs .65 I would like to see a different
surface finish (Immersion Silver?). What do you guys think?
2. Solder Paste. I have used type 4 powder mesh size (-400+635) in the
past but not much success. Who has had success with type 4 and who was
the vender?
3. Stencil Apertures. I know the industry recommends 4 to 5 mil stencil
for this application but what other techniques have you "wizards" tried
in the past? I have tried step downs, dog bones, bow tie, home base
plate, 10% and 20% reductions and various combinations. My biggest
concern is developing the process and stencil around the 16 mil
component. I also have seen success with Nickle plated aps to aid with
release for the super fine pitched devices.

Thanks in advance guys and gals!!

Carl Ray
Sr. Manufacturing Engineer
Huntsville, AL 35807
Phone: 256-882-4800 ext. 8845
Cell: 256-990-1990

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------



 ========================================================================
DISCLAIMER:
The information contained in this communication is confidential and may be legally privileged.
It is intended solely for the use of the individual or entity to whom it is addressed and others
authorized to receive it. If you are not the intended recipient, you are hereby notified that any
disclosure, copying, distribution, or taking any action in reliance of the contents of this information
is strictly prohibited and may be unlawful. Stork is neither liable for the proper and complete
transmission of the information contained in this communication nor for any delay in its receipt.


---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2