Have you tried solder manufacturers' web sites?
For sure there is a shortened version of our Solder Alloys Directory on
ours. IF the alloys you want are sufficiently obscure you can ask for the
full 220 alloy listing to be sent to you.
www.Google.com will also answer in 0.something seconds, but be sure to ask a
directed question or it will bury you:)
Regards
Mike Fenner
Applications Engineer, European Operations
Indium Corporation
T: + 44 1908 580 400
M: + 44 7810 526 317
F: + 44 1908 580 411
E: [log in to unmask]
W: www.indium.com
Leadfree: www.Pb-Free.com
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of sahmad
Sent: Thursday, February 13, 2003 9:50 PM
To: [log in to unmask]
Subject: [TN] Solder CTEs
I have seen solder composition tables with their melting point. Is there a
listing of their CTEs?
Thanks.
Syed.
Syed Sajid Ahmad
Advanced Packaging Technology/Fab 4
Mail Stop 718
Micron Technology, 8000 S. Federal Way, Boise ID 83716-9632
(208)368-3359 Fax (208)363-2994
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|