Wee Mei,
To the first question:
The best is to get the components with legs of the proper length. Otherwise,
the legs should be trimmed. It is better than short to the body.
However, the trimming should be done before the soldering, because
1. Trimming after the soldering will leave exposed copper, and
2. The shock of the cut of thick legs will cause cracks in the soldering.
This is true whether you are using hand cutter or motorized surcace cutter.
To the second question:
Yes, it is possible; however, do not forget to consider the heat of the
resistor: It may affect the adhesive long term strength, and if the adhesive
blocks the air around it it may ovrheat.
Regards
Ofer Cohen
Quality Assurance Manager
SEABRIDGE Ltd.
> -----Original Message-----
> From: Lum Wee Mei [mailto:[log in to unmask]]
> Sent: Friday, February 14, 2003 02:03
> To: [log in to unmask]
> Subject: [TN] Lead Trimming & Gluing components
>
>
> Hello,
>
> I have 2 questions to ask : "Are we allow to trim down the
> leads of the
> power module after assembly just because they will touch the chassis
> cover?" & "Are components such as power resistors allowed to
> be soldered via wires to the PCBs and tab down on the PCBs with
adhesives?"
>
> To me, leads from connectors, power modules are not supposed to be
> trimed regardless before or after assembly. Then I may be wrong.
>
> Any advice out there?
>
> Thanks and regards,
> Wee Mei
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using
> LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with
> following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send
> e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail
> to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm
> for additional
> information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|