TECHNET Archives

February 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
James TerVeen <[log in to unmask]>
Date:
Wed, 12 Feb 2003 11:10:47 -0500
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Bissonnette, Jean-Francois" <[log in to unmask]>
Subject:
From:
"Bissonnette, Jean-Francois" <[log in to unmask]>
X-cc:
"Technet (E-mail)" <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (157 lines)
I'll see what I can do for the pictures.  

The cracking are near the end terminasion.  They are called "flex-cracks"
apparently due
to flex of the boards but the boards they're soldered on are rather thick
we're not sure.
And there is a variety of reasons why these appeared.  What we're facing now
is more 
can we do it another way so these cracks are not appearing?  The TH part
seems to be
the most economical way, on short term that is.  But I've seen more than
enough situation
where economical way turn out to be "pay now or pay (more) later".  

I want to know if anyone tried it the way I said before and what they came
up with.

Here is a link to a report on these cracks.  It may interest some of the
technetters.

http://www.syfer.com/ta_02.htm

-----Original Message-----
From: James TerVeen [mailto:[log in to unmask]]
Sent: Wednesday, February 12, 2003 10:48 AM
To: TechNet E-Mail Forum.; Bissonnette, Jean-Francois
Subject: Re: [TN] TH capacitor on SMT pads



I guess coming from a Chip manufacturers side I need to ask Why you do not
change suppliers.   What kind of cracking are you talking about.  I ask
this because I just did a long process of tracking down a cracking problem
with a customer and the final result was they had to much pressure in
placing the component and were cracking it there.   Very small cracks but
they were there and when they fired up the board the cracks got much
larger.   Can you supply a picture of the cracks to Steve so we can take a
look.


 

                      "Bissonnette,

                      Jean-Francois"           To:       [log in to unmask]

                      <JBissonnette@WAB        cc:

                      TEC.COM>                 Subject:  [TN] TH capacitor
on SMT pads                     
                      Sent by: TechNet

                      <[log in to unmask]>

 

 

                      02/12/03 10:24 AM

                      Please respond to

                      "TechNet E-Mail

                      Forum."; Please

                      respond to

                      "Bissonnette,

                      Jean-Francois"

 

 





Hi Technetters,

We're having problem with some multilayer ceramic capacitors (SMT), they
crack.  We have a
high level of rejects from the field and we're thinking of replacing them.
However, the
best that the design team came up with so far is to use regular ceramic
capacitor (TH)
(... please don't ask why they don't chance supplier... I already did and
well, forget it!)

I'm not too confortable with that, but on the other hand, a design change
on
the board
would be very costly and we want to avoid that.

Did anyone ever changed a SMT part for a TH part?  What problems should we
expect
if we decide to go that way?  Of course assuming that the leads would be
bent properly, the
cap would be bonded to the board, every applying rule for soldering would
be
respected and
Murphy won't show its ugly face... then again we all know what appends when
we assume...

I'd prefer to go another way but my way will cost a lot of money and I'm
told that we have to
keep it to a minimum.

Any thoughts?

Jean-François Bissonnette
Vérificateur, Contrôle de la Qualité
Électronique



***** CONFIDENTIALITY NOTE *****
The content contained in this e-mail transmission is legally privileged and
confidential information intended only for the use of the individual or
entity named herein. If the reader of this transmission is not the intended
recipient, you are hereby notified that any dissemination, distribution, or
copying of this transmission is strictly prohibited.

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------





***** CONFIDENTIALITY NOTE *****
The content contained in this e-mail transmission is legally privileged and confidential information intended only for the use of the individual or entity named herein. If the reader of this transmission is not the intended recipient, you are hereby notified that any dissemination, distribution, or copying of this transmission is strictly prohibited.

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2