Dave: You may want to look into Mixed Flowing Gas (MFG) testing. This uses
trace amounts of corrosive gases to simulate various environments such as
water treatment, refinery, industrial storage, etc. They provide an
accelerated test for corrosion stress. It is usually done with Cu, however
it may be of value in pointing up any weaknesses in your coating and
possibly provide comparative information if not quantifiable. Battelle has
done quite a bit of work in this area that resulted in various classes,
methods and correlation data for MFG testing.
Although the aluminum does form a fairly un-reactive oxide, in the right
chemistry and environmental conditions it could be a problem.
Do you need to form an electrical ground to the chassis? If so there are
limitations to the quality of ground. In some cases we have ended up tin
plating the aluminum chassises.
Regards
Michael Barmuta
Staff Engineer
Fluke Corp.
Everett WA
425-446-6076
-----Original Message-----
From: Dave Hillman [mailto:[log in to unmask]]
Sent: Tuesday, February 04, 2003 12:12 PM
To: [log in to unmask]
Subject: [TN] Galvanic Corrosion Testing
Hi TechNet! I am on a quest for some information and hoping the minds of
TechNet can send me charging off in the right direction. Rockwell Collins
has been very active in implementing the new immersion pwb finishes
(immersion tin, immersion silver, ENIG). The implementation has been very
successful with few "bumps in the road" being encountered. However, one
question has arisen that; a) as a metallurgical engineer I should have
anticipated and b) you would think someone else would have solved already.
The question is " Is there a galvanic corrosion issue with the use of
either ENIG or immersion silver pwb surface finishes and the aluminum
chassises/enclosures"? As background, there is very little of the pwb
finish in intimate contact with the aluminum chassis with most of the
contact being aluminum standoff posts contacting a circular mounting pad on
the pwb. I have spent a number of hours looking for some type of galvanic
corrosion test which I could run to determine if either immersion silver or
ENIG finishes would be an issue. The two environments I have the most
interest in are temperature/humidity and salt air. I am tentatively going
to run an 85C/85%RH and an ASTM salt fog exposure on some mockup test sets
to see if I have any reactions. Has anyone run such a test or can anyone
direct me to a Mil STD or ASTM standard which deals with galvanic corrosion
of contacting dissimilar metals?
Thanks in advance.
Dave Hillman
Rockwell Collins
[log in to unmask]
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|