Anyone had success using wash-away spacers during wave-soldering, then
removing them by aqueous cleaning? We're looking at them mostly to
control standoff of transistor cans and vertically-mounted resistors.
Looking at the Bivar catalog, spacers come in two types, normal and
"effervescent", which dissolve more quickly.
Do they wash away completely? Leave any residue that affects conformal
coat adhesion? Any problems with the materials reacting with the wash
chemistry, either saponifier or alcohol based?
Joe Kane
BAE SYSTEMS Controls
Johnson City, NY
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|