Hi Bev,
As an option, you might look at  http://www.ormetcircuits.com/ . In fact,
maybe you are familiar with the process since they reference Nortel
qualification.

Mel Parrish
Director, Training Materials Resources
Soldering Technology International
102 Tribble Drive
Madison, AL 35758
256 705 5530
256 705 5538 Fax
[log in to unmask]
www.solderingtech.com

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Bev Christian
Sent: Thursday, January 16, 2003 1:01 PM
To: [log in to unmask]
Subject: [TN] Purposefully shorting two adjacent SOIC leads.


Technetters,
How do I do what is proposed in my title?  The options are using excess
solder or using a mod wire.  Are there other options for doing this mod?
What do people do?  What is allowed and not allowed by IPC standards (I
couldn't find anything, but then I may not be looking in the right place.)
I would expect option one would be a whole heck of a lot easier than option
2.  As long as option 1 doesn't produce bulbous joints with the solder all
the way up to the component body is there any real reason why I can't do
this?

regards,
Bev Christian
Research in Motion

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2