At 09:27 AM 1/29/2003 +0100, Zweigart, Siegmund wrote:
> Hello all
>
>We got a request from a potential customer regarding high frequency
>materials.
>The frequency on the product will be 24- 26 GHz.
>Is there a mainstream PCB base material for this frequencies?
Lot's of choices. But the answer as always is "it depends" on your specific
application.
Need to consider a number of factors including:
1. degree of material stability and rigidity required (many uwave
dielectrics are unsupported, unstable dimensionally and unreliable in
multilayer stackups)
How large an image will it be?
Will it be a simple doublesided board or a multilayer?
2. Low or high power? Is thermal dissipation critical?
3. Does the designer have an idea how low a loss tangent is desired/required?
4. Is higher or lower Dk (Er) preferred by the EE?
Dwight
>What are the pro and cons of the different materials?
>Any feedback is welcome.
>
>Best regards
>
>Siggi
>
>---------------------------------------------------
>Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
>information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
>ext.5315
>-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|