IPC-A-610C 3.4.5 states the Target condition for Class 1,2,3 is to handle with gloves.
Acceptable condition is to handle the boards by the edges.
We handle all boards by the edges UNLESS otherwise specified by our customer. We do have one customer which is class 3 and requires we handle the boards with gloves AFTER the last cleaning operation.
-Carrie
-----Original Message-----
From: Stolar, Paul W [mailto:[log in to unmask]]
Sent: Friday, January 10, 2003 3:21 PM
To: [log in to unmask]
Subject: [TN] Gloves-Poll
Most electronics mfg places I have seen require gloves or finger cots to be
worn when handling assemblies.
Does your place require gloves or finger cots, or just trust the people to
not smudge the boards?
Paul Stolar
Materials Engineer
Baker Atlas
713-625-5376
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|