Mark,
You need to ask your mechanical engineer what is the limiting feature in the
design.
If you have wrap around end launch connectors or a card guide, then it might
be the laminate. If you have a case going over the assembly, which might
interfere with components, then it might be the over the copper, excluding
solder if you hand solder, including solder otherwise. If a gull wing
surface mount connector sits on the Soldermask, then perhaps you need to
control the thickness over the Solder mask.
My quick review of 6012 did not find a 'default' definition of overall
thickness.
Over the years, I have often been surprised at what I got, when I didn't
know what I asked for. I call them 'lessons learned'.
Best Regards,
George Franck
"My opinions are just that."
====================
Hi All,
Here's what was ordered:
0.062" finished board thickness, SMOBC, HASL final finish, IPC-6012 class 2.
Here's the question:
Does finished board thickness include the HASL coating thickness?
Thanks,
Mark Hargreaves
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|