Hi Bill,
Has the manufacturer changed the material the components are made from?
Steve.
-----Original Message-----
From: Bill Page [mailto:[log in to unmask]]
Sent: 22 January 2003 15:09
To: [log in to unmask]
Subject: [TN] This is a new one on me
Hey folks,
I've been in this business for over 20 years, and thought I had seen it all,
but this is a new one. We're having problems with our glue/wave solder
process. Parts are falling off the board.
"That's not new," you say?
"Check your handling, stupid," you say?
"Check your glue cure process, stupid," you say?
Yep.
Shear tests indicate that our glue process is working.
We're using a product that is very widely used in the industry, following
the manufacturer's recommended cure profile.
And yet, parts fall off -- as they go through the wave solder machine.
Adhesive stays put. Has a flat surface where the part used to be.
Pads are beautifully soldered...just no parts there.
And we have verified that the parts are present before the wave.
Across chip suppliers and part numbers, across solder mask types, across PWB
vendors.
Is it just me?
Is the business finally catching up with me?
Should I give up and become a high school band director?
Your suggestions are welcome!
Bill Page
Kenosha, WI
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
________________________________________________________________________
This e-mail has been scanned for all viruses by Star Internet. The
service is powered by MessageLabs. For more information on a proactive
anti-virus service working around the clock, around the globe, visit:
http://www.star.net.uk
________________________________________________________________________
_____________________________________________________________________
This message has been checked for all known viruses by Star Internet delivered
through the MessageLabs Virus Control Centre.
__________________________________________________________________________
Disclaimer of Liability
ATL Telecom Ltd shall not be held liable for any improper or incorrect use of the information described and/or contained herein and assumes no responsibility for anyones use of the information. In no event shall ATL Telecom Ltd be liable for any direct, indirect, incidental, special, exemplary, or consequential damages (including, but not limited to, procurement or substitute goods or services; loss of use, data, or profits; or business interruption) however caused and on any theory of liability, whether in contract, strict liability, or tort (including negligence or otherwise) arising in any way out of the use of this system, even if advised of the possibility of such damage.
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|