Bev,
In my experience, shorting adjacent legs on an SOIC is a reliable and
effective way of making this modification. Because the legs are so close to
each other there is little relative movement so no force to disrupt the
joint.
In a similar vein, I have also developed what I call a "solder slink". This
makes a zero ohm link between adjacent pads without the aid of a zero ohm
resistor. They are formed during the normal paste/place/reflow cycle only
nothing is placed. If you need to change to the next connection, a few
seconds with an iron, some solder wick and fresh solder wire and it's done.
I can send details if anybody is interested.
My only reservation about the SOIC mod. is when a customer sees it for the
first time and thinks that a manufacturing error has occurred. As long as
the customer is happy and understands I believe it is the best way to go.
Regards
Eric Dawson
> -----Original Message-----
> From: Bev Christian [SMTP:[log in to unmask]]
> Sent: Thursday, January 16, 2003 7:01 PM
> To: [log in to unmask]
> Subject: [TN] Purposefully shorting two adjacent SOIC leads.
>
> Technetters,
> How do I do what is proposed in my title? The options are using excess
> solder or using a mod wire. Are there other options for doing this mod?
> What do people do? What is allowed and not allowed by IPC standards (I
> couldn't find anything, but then I may not be looking in the right place.)
> I would expect option one would be a whole heck of a lot easier than
> option 2. As long as option 1 doesn't produce bulbous joints with the
> solder all the way up to the component body is there any real reason why I
> can't do this?
>
> regards,
> Bev Christian
> Research in Motion
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> -----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|