TECHNET Archives

January 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
Virgil Lenton <[log in to unmask]>
Date:
Thu, 16 Jan 2003 12:43:18 -0600
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Virgil Lenton <[log in to unmask]>
Parts/Attachments:
text/plain (29 lines)
I apologize for the vagueness in my original posting.
This is what we know so far about this problem.

- It does not appear to be Z-height related - nozzles are spring loaded and
we have double checked.
- Breaks are complete breaks through the center of the body. Sometimes
the 'lid' comes off, but most often they crack top to bottom right through.
- We have *not* explored the possibility of moisture, but at this pont we
feel moisture is unlikely.
- The components in question are all placed on pass 1. We havent yet
checked to see if they are cracked before pass 2.
- It is not always the same part, but always SOT-23.
- The profile used is our 'standard' profile that has been used for about 3
years.

Regards
Virgil

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2