Bonjour Yannick!
Thermal mass is not an accurate term, but is widely used as it seems to be something people can easily understand. If I say to you that this heavy part will absorb more heat it sounds reasonable. The profile results are a result of many factors including how heavy / dense components are, how thick the PWB is, what oven you are using, surface finishes on components... much more than just the weight.
There is no easy calculation, the only way I know of to be sure you have the right profile is to hook thermocouples to the board and run some trials. You must use thermocouples on both the smallest and most exposed parts, as well as the heaviest and most shadowed parts.
Good luck!
regards,
Graham Collins
Process Engineer,
Northrop Grumman Canada Corporation
Halifax
(902) 873-2000 ext 6215
>>> [log in to unmask] 01/15/03 01:09PM >>>
Hi,
For quiet long I've heard people said that the reflow profile must be
change for each board depending of the thermal mass of the board. My
question is how do you calculate this Thermal mass? Or to have a good
profile do you take all the datasheet of the component on the board and take
an average of that?
Hope you can help me with this issue.
Thanks You
Yannick Brisson
============================
Technicien SMT
Technician SMT
M2S Électronique
2855, Rue de Celles
Québec, Québec
G2C 1K7
Téléphone: (418) 842-1312 Ext: 264
Télécopie: (418) 842-0123
[log in to unmask]
============================
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|