TECHNET Archives

January 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Tue, 14 Jan 2003 11:34:08 -0500
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Content-type:
text/plain; charset=iso-8859-1
Subject:
From:
Marcus Wheeler <[log in to unmask]>
X-cc:
Content-transfer-encoding:
quoted-printable
MIME-Version:
1.0
Parts/Attachments:
text/plain (247 lines)
 In the Contract Mfg. environment there are multiple process's going on in
the same shop some are customer driven some our left up to our discretion.
In our shop we have VOC free flux -alcohol based No-clean- and OA wave
soldering flux as well as 3 different types of solder paste. Our designers
can not be sure which process the PCB's will be run. Maybe in an OEM
environment what you say is true.

Marcus Wheeler
Sr. Mfg. Engineer
Apsco International
[log in to unmask]
440-352-8961 * 530



                                                                                                                       
                      joyce                                                                                            
                      <[log in to unmask]        To:       [log in to unmask]                                               
                      OM>                      cc:                                                                     
                      Sent by: TechNet         Subject:  Re: [TN] Stencils                                             
                      <[log in to unmask]>                                                                                
                                                                                                                       
                                                                                                                       
                      01/14/2003 11:18                                                                                 
                      AM                                                                                               
                      Please respond to                                                                                
                      joyce.koo                                                                                        
                                                                                                                       
                                                                                                                       




Are you telling me the MFG is selecting the paste now instead of the
design house?  I thought material change is a major change, that
including the flux type used for the process.  The designer better be
fully aware of the following:
(1) environmental operation condition and reliability (pad size and
filler size included)
(2) subsequent reliability issue related to the possible residue left on
the board (water soluble or no clean)
(3) components lead finishing and shelf life issue related to the flux
used and hopefully, different source of components terminal finishing
vs.. flux/process used (someone should take a overall responsibility if
it is not designer = personally, I think he should be the one, since he
is the one to select the components.  We are not talking about the
draftsmen here).
Go back to the old argument now: send your designer walk the floor for
3-6 month (if you got Union to prevent him actually do the hands on) and
make sure he understand the issues before doing design.
My 1.28 cents.
                                                   jk

>-----Original Message-----
>From: TechNet [mailto:[log in to unmask]] On Behalf Of Marcus Wheeler
>Sent: Tuesday, January 14, 2003 10:50 AM
>To: [log in to unmask]
>Subject: Re: [TN] Stencils
>
>
> The board designer has no idea which process the PCB will be
>run i.e. water soluble vs noclean. The stencils for a
>water-soluble paste would less likely include home plate and
>other aperture modifications. Therefore it is my opinion that
>it must ultimately be the Mfg, Engineer 's job designing the
>actual stencil.
>
>Marcus Wheeler
>Sr. Mfg. Engineer
>Apsco International
>[log in to unmask]
>440-352-8961 * 530
>
>
>
>
>
>                      "Cyker, Howard A
>
>                      (Howie)"                 To:
>[log in to unmask]
>                      <[log in to unmask]        cc:
>
>                      >                        Subject:  Re:
>[TN] Stencils
>                      Sent by: TechNet
>
>                      <[log in to unmask]>
>
>
>
>
>
>                      01/14/2003 10:16
>
>                      AM
>
>                      Please respond to
>
>                      "TechNet E-Mail
>
>                      Forum."; Please
>
>                      respond to
>
>                      "Cyker, Howard A
>
>                      (Howie)"
>
>
>
>
>
>
>
>
>
>
>I agree with Mr. Croslin with supplying a 1:1 stencil layer
>artwork to the EMS provider so they can tailor the stencil
>design to their materials and assembly processes.  One other
>consideration during stencil design is attachment reliability
>requirements.  If the board designer has specific solder
>volume requirements (beyond industry (IPC) solder joint quality
>standards) to meet product reliability requirements, then
>these requirements must be communicated to the EMS provider
>for consideration when they design the stencil.
>
>
>
>Howard A. Cyker
>Lucent Technologies
>Engineering Infrastructure - New Product Engineering
>
>   Email [log in to unmask]
>   Phone 978-960-2964
>   Fax 978-960-2964
>   Pager 888-961-2336
>
>
>-----Original Message-----
>From: Croslin, Robert [mailto:[log in to unmask]]
>Sent: Tuesday, January 14, 2003 9:58 AM
>To: [log in to unmask]
>Subject: Re: [TN] Stencils
>
>
>From a design standpoint, we provide our CEM houses with a
>one-to-one stencil layer embedded in our Gerber files.  This
>allows them to adjust it appropriately based on their
>equipment, processes, stencil manfacturer, etc.
>
>
>Bob Croslin
>
>Nielsen Media Research
>-----Original Message-----
>From: Donald Kyle [mailto:[log in to unmask]]
>Sent: Tuesday, January 14, 2003 9:33 AM
>To: [log in to unmask]
>Subject: [TN] Stencils
>
>
>I would like your opinion on who would be more suited to
>design stencils for SMT PWBs; the board designer or the
>contract-manufacturing engineer.
>
>What do you do and why?
>
>
>
>
>Donald Kyle C.I.D.+
>281-285-7528 ---------------------------------------------------
>Technet Mail List provided as a free service by IPC using
>LISTSERV 1.8e To unsubscribe, send a message to
>[log in to unmask] with following text in the BODY (NOT the
>subject field): SIGNOFF Technet To temporarily halt or
>(re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at:
>http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/html/forum.htm for additional information, or contact
Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------



---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/html/forum.htm for additional information, or contact
Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------




---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
 -----------------------------------------------------



---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2