TECHNET Archives

January 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Tue, 14 Jan 2003 11:13:22 -0500
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Cyker, Howard A (Howie)" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="ISO-8859-1"
From:
"Cyker, Howard A (Howie)" <[log in to unmask]>
Parts/Attachments:
text/plain (178 lines)
Marcus,

You and I are already in agreement, the manufacturing engineer (EMS) must
design the stencil.  However, if the board designer has specific solder
volume requirements to meet solder joint attachment requirements (for
certain components), then those volume requirements must be communicated to
the manufacturing engineer to be incorporated into the stencil design.

Howard A. Cyker
Lucent Technologies
Engineering Infrastructure - New Product Engineering
        Email [log in to unmask]
        Phone 978-960-2964
        Fax 978-960-2964
        Pager 888-961-2336



-----Original Message-----
From: [log in to unmask] [mailto:[log in to unmask]]
Sent: Tuesday, January 14, 2003 10:50 AM
To: TechNet E-Mail Forum.; Cyker, Howard A (Howie)
Subject: Re: [TN] Stencils



 The board designer has no idea which process the PCB will be run i.e.
water soluble vs noclean. The stencils for a water-soluble paste would less
likely include home plate and other aperture modifications. Therefore it is
my opinion that it must ultimately be the Mfg, Engineer 's job designing
the actual stencil.

Marcus Wheeler
Sr. Mfg. Engineer
Apsco International
[log in to unmask]
440-352-8961 * 530



 

                      "Cyker, Howard A

                      (Howie)"                 To:       [log in to unmask]

                      <[log in to unmask]        cc:

                      >                        Subject:  Re: [TN] Stencils

                      Sent by: TechNet

                      <[log in to unmask]>

 

 

                      01/14/2003 10:16

                      AM

                      Please respond to

                      "TechNet E-Mail

                      Forum."; Please

                      respond to

                      "Cyker, Howard A

                      (Howie)"

 

 






I agree with Mr. Croslin with supplying a 1:1 stencil layer artwork to the
EMS provider so they can tailor the stencil design to their materials and
assembly processes.  One other consideration during stencil design is
attachment reliability requirements.  If the board designer has specific
solder volume requirements (beyond industry (IPC) solder joint quality
standards) to meet product reliability requirements, then these
requirements must be communicated to the EMS provider for consideration
when they design the stencil.



Howard A. Cyker
Lucent Technologies
Engineering Infrastructure - New Product Engineering

   Email [log in to unmask]
   Phone 978-960-2964
   Fax 978-960-2964
   Pager 888-961-2336


-----Original Message-----
From: Croslin, Robert [mailto:[log in to unmask]]
Sent: Tuesday, January 14, 2003 9:58 AM
To: [log in to unmask]
Subject: Re: [TN] Stencils


From a design standpoint, we provide our CEM houses with a one-to-one
stencil layer embedded in our Gerber files.  This allows them to adjust it
appropriately based on their equipment, processes, stencil manfacturer,
etc.


Bob Croslin

Nielsen Media Research
-----Original Message-----
From: Donald Kyle [mailto:[log in to unmask]]
Sent: Tuesday, January 14, 2003 9:33 AM
To: [log in to unmask]
Subject: [TN] Stencils


I would like your opinion on who would be more suited to
design stencils for SMT PWBs; the board designer or the
contract-manufacturing engineer.

What do you do and why?




Donald Kyle C.I.D.+
281-285-7528 ---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------



---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2