Steve,
We reuse our solder paste. Whenever paste is removed from the stencil, it is put in it's own jar. Never mix the old paste into the fresh jar. Another thing we use is the 250 gram jars instead of the big 500 gram jars. We feel it minimizes the amount of time it's being opened. We do toss any opened paste at the end of the shift.
-Larry Koens-
-----Original Message-----
From: Steve Gregory [mailto:[log in to unmask]]
Sent: Monday, December 02, 2002 7:35 PM
To: [log in to unmask]
Subject: [TN] Solderpaste life...
Hi all!
Hope everybody had a good thanksgiving holiday (our USA members anyway), but have a question about solderpaste life.
We are a low-volume, high mix shop, and we may run 5-20 assemblies, then switch over to another assembly. The solderpaste between these switch-overs may change from a high activity OA to a low activity no-clean depending on the requirements called out on the assembly drawing.
In the past, we have chosen the path, that once solderpaste is opened, it is either used, or scrapped. But looking closely at this policy, we're throwing a lot of paste away, and maybe we shouldn't.
It's no small change, when I've looked at how much we throw away...just wondering now, and I understand the issues of using very old solderpaste, and mixing fresh with new, but does anybody have any guidelines of when they throw paste away, or put it back in the jar to reuse?
I'm about to write some procedures concerning this. I don't think that once the jar, or container is opened, it needs to be consumed all at once, or scrapped. I do think solderpaste is a bit more robust than that (but you might have a hard time for the vendors to say that...hehehe....sorry Mike!). I do think that if good control is maintained, solderpaste can perform as advertised, whether it has been opened previously or not...
Just curious if anybody else has encountered this issue...and adressed it.
-Steve Gregory- --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|