> Hello fellow Technetters:
>
> Anyone have any experience removing paralyne (paraxylene) coated BGAs and
> uBGAs with conventional air vac DRS 24 type hot air equipment - I tried
> conventional reflow profiles and it was very unsuccessful.
>
> [log in to unmask]
Mike
One other point about reworking is - are you sure that the component will
not be de-graded during this operation...especially if you expose it to
around 200 DegC and levering!?
Furthermore, what is the application for this assembly? Will someone die if
it fails?
If the answer is yes - then scrap the assembly.
You might then want to consider having a coating that is repairable - by
easier means than described.
--
Regards, Graham Naisbitt
[log in to unmask]
Mobile: +44 (0)79 6858 2121
Concoat Limited - Engineering Electronics Reliability
Web: www.concoat.co.uk AND www.concoatsystems.com
NOTE: NEW ADDRESS :NOTE
Sales:
Millfield House, Fleet Road
Fleet, Hampshire GU51 3QF UK
Phone: +44 (0)1252 813706
Fax: +44 (0)1252 813709
Manufacturing and Head Office:
Alasan House, Albany Park
Camberley, Surrey GU16 7PH UK
Phone: +44 (0)1276 691100
Fax: +44 (0)1276 691227
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|