Peter,
Yes sir, reflow. So that would include the HASL or maybe plate-reflow,
initial solder, possibly a reflow cycle if mixed. Then the rework could
include solder extraction/removal, site preparation, resolder. All in all,
that's quite a lot to expect from the materials. Each operation is
cumulative and can impact the next, even if accomplished carefully and
skillfully. I have to admit that participating in some studies that included
rework cycles that were continued until the product became unsolderable or
materially failed and there were commonly 5-8 cycles as I recall before that
happened . Still would not recommend nor expect that performance today. I
didn't include bake out or ESS since that didn't elevate the temperature to
solder melt temperatures even though they can significantly contribute to
intermetalic growth and inherent solderability issues.
Best wishes for a wonderful Christmas season.
Mel Parrish
Director, Training Materials Resources
Soldering Technology International
102 Tribble Drive
Madison, AL 35758
256 705 5530
256 705 5538 Fax
[log in to unmask]
www.solderingtech.com
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of
[log in to unmask]
Sent: Thursday, December 19, 2002 6:24 PM
To: [log in to unmask]
Subject: Re: [TN] PCB Repair Criteria
Mel,
What's your interpretation of the 5 thermal cycles - do they include the
thermal cycling used to fabricate the PCB in the first place? And what
temperatures are we talking about? Does, say, a bake cycle at 90 degrees
count, or are we talking reflow temperatures? Just curious.
Peter
Mel Parrish <[log in to unmask]> 19/12/2002 11:16 PM
Sent by: TechNet <[log in to unmask]>
Please respond to "TechNet E-Mail Forum."; Please respond to Mel Parrish
To: [log in to unmask]
cc: (bcc: DUNCAN Peter/Asst Prin Engr/ST Aero/ST Group)
Subject: Re: [TN] PCB Repair Criteria
Much of the ability to survive rework or thermal excursions is dependent
upon the fabrication materials. The board qualification criteria under the
55110 was designed around 5 thermal cycles, which if you add them up, gives
you one rework process if it requires extraction and site preparation.
After
that all bets are off. The qualification other than 55110 is less robust
so
you can see what you might be up against.
Good Luck, Mel
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Victor Hernandez
Sent: Thursday, December 19, 2002 8:34 AM
To: [log in to unmask]
Subject: Re: [TN] PCB Repair Criteria
The repair site is a Power FET on a .062 PCB with 4 layers. This is the
Vcore plane. Perhaps 1oz.
victor,
-----Original Message-----
From: Charles Caswell [mailto:[log in to unmask]]
Sent: Thursday, December 19, 2002 8:30 AM
To: [log in to unmask]
Subject: Re: [TN] PCB Repair Criteria
This is a difficult question to answer. The simple answer is none.There are
too many factors involved. Lead to hole ratio, copper weight, skill of
operator and equipment used are all variables to consider. I have removed
and replaced a 172 pin PGA 15 times in a 15 layer board with no apparent
damage. Although I'm sure there was some degradation to the life expectancy
of the board. This board was later used as part of the flight
qualification,
-40 to +85 degC severe vibe etc. and passed. I will be watching for other
replies to this one.
Charles Caswell
-----Original Message-----
From: Victor Hernandez [mailto:[log in to unmask]]
Sent: Thursday, December 19, 2002 7:55 AM
To: [log in to unmask]
Subject: [TN] PCB Repair Criteria
> Fellow TechNetters,
>
> Can some one assist me with this question. How man times can a
PTH
> component be
safely removed before damage to the inner connections on the barrel occurs.
> Victor G. Hernandez
>
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|