I did not give any details as I wanted to understand all the possibility
which could contribute to via cracking. Does anyone have white papers on the
subject?
Assuming the boards were made correctly, what in the manufacturing process
could contribute to this defect. From the report it is mainly occuring near
ICs (QFPS, SOICs).
-----Original Message-----
From: Werner Engelmaier [mailto:[log in to unmask]]
Sent: Tuesday, December 03, 2002 2:42 PM
To: [log in to unmask]
Subject: Re: [TN] via cracking
Hi Dennis,
Via barrel cracking typically--you do not give any details--occurs as the
result of the much larger thermal expansion of the resin surrounding the via
than the copper of the barrel during soldering processes. There are
contributing factors, i.e. PWB design, hole quality, barrel copper quality,
resin content, etc.
I give a one-day workshop on this [see outline at website].
Werner Engelmaier
Engelmaier Associates, L.C.
Electronic Packaging, Interconnection and Reliability Consulting
7 Jasmine Run
Ormond Beach, FL 32174 USA
Phone: 904-437-8747, Fax: 904-437-8737
E-mail: [log in to unmask], Website: www.engelmaier.com
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
Scanned by PeNiCillin http://safe-t-net.pnc.com.au/
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|