Fellow Technet subscribers,
I have a question related to BGA standoff distance after reflow. We are
noticing some variation in standoff distance on some of the larger plastic
BGAs installed onto densely populated, double sided boards. By standoff
distance I mean the distance measured between the bottom of the BGA package
and the top of the solder mask located on the pwb.
Is standoff distance considered a good indicator of correct solder ball
collapse? Is there a formula for calculating what the theoretical standoff
distance should be after reflow based on package weight, solder ball
diameter, # of balls, etc...?
Joe
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|