TECHNET Archives

December 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Content-Type:
text/plain; charset="ISO-8859-1"
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>
Date:
Mon, 9 Dec 2002 14:13:00 -0800
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Rick Thompson <[log in to unmask]>
Subject:
From:
Rick Thompson <[log in to unmask]>
Content-Transfer-Encoding:
7bit
Sender:
Parts/Attachments:
text/plain (31 lines)
Hi,

Does anyone have any experience they'd be able to share regarding using
no-clean wave solder flux with selective solder fixtures?  We've found that
the flux tends to wick under the edge of the fixture, and does not fully
harden on exposure to the wave.  I suspect this is due to not reaching a
high enough temperature.  Has anyone seen this phenomenom? We are preheating
the board per our current flux vendor's recommendations.  Any
recommendations as to corrective actions we could look at?  Flux
recommendations (offline please)?

Thanks in advance,

Rick Thompson

Sr. SMT Process Engineer
SMTEK International, Inc.
+1 (805) 532-2800
[log in to unmask]

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2