I also pick "A" and I think I will be serving it at my
Thanksgiving feast.    It should be very tasty and the
Women we probably really enjoy it

Thanks



                      dopauls@ROCKWELLC
                      OLLINS.COM               To:       [log in to unmask]
                      Sent by: TechNet         cc:
                      <[log in to unmask]>        Subject:  Re: [TN] Purple plague


                      11/27/02 09:12 AM
                      Please respond to
                      "TechNet E-Mail
                      Forum."; Please
                      respond to
                      dopauls






Ioan,

Regarding purple plague:

a.  Purple Plague
1 1/2 oz Chambord raspberry liqueuer
4 oz white wine (Zinfandel)
3 splashes 7-up

b.  an ordnance survey in England

c.  A photographic problem

d.  http://www.corrosion-doctors.org/MatSelect/corrgold.htm

e.  an invasive plant also called purple loosestrife

Personally, choice A seems appealing right about now...................

Doug Pauls
Advanced Operations Engineering
Rockwell Collins



                      "Tempea, Ioan"
                      <itempea@POSITRON        To:       [log in to unmask]
                      .QC.CA>                  cc:
                      Sent by: TechNet         Subject:  [TN] Purple plague
                      <[log in to unmask]>


                      11/27/02 07:34 AM
                      Please respond to
                      "TechNet E-Mail
                      Forum."; Please
                      respond to
                      "Tempea, Ioan"






Hi Technos,

after flirting with black pads, I remembered having read something about
purple plague. Can anybody point me to on-line documentation on the purple
plague?

Thank you,
Ioan

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
 -----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2