We tried several boards with immersion tin from different vendors.
Some of them had very good solderability, others not.The soldering
conditions were the same as for hot air leveling.
We tried to see where the problem was, and saw that the problem occured
mostly on boards which were plugged BEFORE the mmersion tin plating, only on
one side. The same problem was seen on immersion silver boards which were
plugged before the final finish, and on these we run a contamination test
which they failed.
IMHO , if the boards are new, it could be a contamination issue due to
contaminants in the vias not being washed away properly because of the
plugging on one side. The interesting point was that the problem was more
visible after the second reflow.
Maybe we ca shed some light on this?
Gaby
----- Original Message -----
From: "Yannick Brisson" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Monday, November 25, 2002 3:03 PM
Subject: [TN] Immersion Tin
> Hi,
>
> I made a board wich I plated with immersion Tin, I tought it should be
the
> same result as we had with tin lead but we ran into a weird problem. We
use
> a 63/37 no clean paste and on the Board with Immersion Tin the solder
just
> make a ball ON the pad...we ran the same profile with a board Tin-Lead and
> we get almost a perfect solder joint. Because it's immersion tin should
we
> put our temperature higher?
>
> We try to solder with a iron and the paste can hardly wet all the pad
the
> fisrt time..if we do it a first time, cleand the pad and do it again it's
> more easy. If someone have work with it can give me some trick I would
> appreciate.
>
> Thanks You
>
> Yannick Brisson
> ============================
> Technicien Ingénierie de Production
> Technician Production ingineering
> M2S Électronique
> 2855, Rue de Celles
> Québec, Québec
> G2C 1K7
> Téléphone: (418) 842-1312 Ext: 264
> Télécopie: (418) 842-0123
> [log in to unmask]
> ============================
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
> -----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|