Permanganate is from the metal - manganese. That is different from
magnesium. Usually, magnesium is a dried on salt from hard water. Is there
calcium in the same area?
While gold is not known to migrate so easily as say copper, silver, or tin.
I suppose it is possible. Gold is elemental on the board, and to get it
ionic to be able to migrate, would take a really strong acid or cyanide ion.
Both seem unlikely. Could the gold have been smeared mechanically - it is
really soft?
Denny Fritz
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------