Hi Rudy: In Gerard's reflow/fusing question he doesn't mention using the hot
oil process, he might be using IR fusing.
In either case as Rudy stated it is usually something upline from the fusing
process.
1. Most Sn/Pb electroplate baths these days are not kept in the best
condition for fusing Sn/Pb, the are usually used as an etch resist bath.
There are many things in the bath that can affect the fusing properties of
the deposit. Some of the most common are organic contamination, improper
current density, trace metal build up (i.e. Cu, Fe, etc) and poorly
controlled bath chemistry.
2. You are probably doing ammoniacal etching of the outerlayers. If the
boards are not properly rinsed and processed thru solder conditioner and
dried they will present fusing problems.
3. Boards should be fused as soon as possible after etching. Long storage
times of the porous electrodeposit will cause oxidation and result in poor
fusing.
4. If you are using IR fusing, the age and Sp. Gr. and application of the
flux are critical. So is the condition, output and cleanliness of the fusing
lamps and reflectors.
Regards
Michael Barmuta
Staff Engineer
Fluke Corp.
Everett WA
425-446-6076
-----Original Message-----
From: Rudy Sedlak [mailto:[log in to unmask]]
Sent: Friday, November 08, 2002 7:01 AM
To: [log in to unmask]
Subject: Re: [TN] need SnPb reflow line resource
I am old enough to have experienced more hot oil reflowing than I care to
relate.
My company published some trouble shooting guides for hot oil reflow...which
are still available to you, or anyone still doing this.
Bottom line, back in the days when we were selling hot oil for reflow, is
that we stopped sampling people fuse oil or flux to solve reflow problems,
because we found they were always caused by things that happened before the
panel went into the oil.
We got pretty good at trouble shooting the pre-fusing process.
I would be happy to discuss the matter with you personally, (650-962-8004)
or send you the trouble shooting guides.
Good Luck
Rudy Sedlak --------------------------------------------------- Technet Mail
List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe,
send a message to [log in to unmask] with following text in the BODY (NOT the
subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery
of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To
receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest Search the archives of previous posts
at: http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/html/forum.htm for additional information, or contact
Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|