Carrie,
>Why Bad Lead? Lead, like ammo, can be useful if used and stored properly.
Just the point I was trying to make.
>Out of curiosity, Anyone of you out on the TechNet changed over to
Lead-Free?
Yes.
>If so, How is it going?
Mas o Menos, overall more good than bad.
>How are your costs?
Just in materials, 10-30% higher since demand is lower for lead free solder
alloys.
>Who absorbed or is absorbing the increased costs?
It's all coming off the bottom line here.
>How do your solder joints look?
NOT like Sn63, the grain is much more pronounced and a good joint has a
duller appearance.
>How's training the inspectors going?
We use peer inspection, and have a small staff so training hasn't been a
issue. I shudder to think hat it would have been like in some of my past
lives with big QA departments.
My unsolicited comment; given the choice I would stick with Tin/Lead solder.
In a larger operation the cost would go directly to the consumer, who would
receive *no* benefit from the change.
Dan
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|