TECHNET Archives

November 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>
Date:
Fri, 15 Nov 2002 12:16:51 -0500
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Morse, Carrie" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
"Morse, Carrie" <[log in to unmask]>
Parts/Attachments:
text/plain (160 lines)
Of course, I would not mind being on that research committee.
I believe implementing the "ESD whacking Stick" may serve a
dual purpose 

-----Original Message-----
From: Steve MacDonald [mailto:[log in to unmask]]
Sent: Friday, November 15, 2002 12:01 PM
To: [log in to unmask]
Subject: Re: [TN] ESD Requirements in SMT Setup Area?


[Sorry, this is not a very technical post, but it is Friday]

Who wants to be on the research committee to develop specifications for "ESD
whacking Sticks?"

Think of the field research.

Operator: "Hey, why'd you hit me, I'm not even in that department?"

QM: "We're broadening the research group."

~ It's lunch time EST.  I digress.

Steve

----- Original Message -----
From: "Morse, Carrie" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Friday, November 15, 2002 11:36
Subject: Re: [TN] ESD Requirements in SMT Setup Area?


> If you wack him with a stiff metal stick that may help in grounding him,
> so, that may also be a feasible solution :)
>
> -----Original Message-----
> From: Steve MacDonald [mailto:[log in to unmask]]
> Sent: Friday, November 15, 2002 11:12 AM
> To: [log in to unmask]
> Subject: Re: [TN] ESD Requirements in SMT Setup Area?
>
>
> Hi Carl.
>
> ESD shoes may not be a bad idea.  Our SMT guy wears them, and while we do
> not require them, we do recommend them.  No straps, no cords, of course if
> he picks his feet up off the floor and rests them on anything thats not
> grounded I have to wack him with a stick. (I'm kidding about that
> part...well, mostly kidding.)
>
> www.lehighsafetyshoes.com
>
> I'm sure there are others.  I dont handle parts, so I don't need them
> myself.  And there may be another solution.  Anyone?
>
>
> Steve
> Mass Design Inc.
>
> ----- Original Message -----
> From: <[log in to unmask]>
> To: <[log in to unmask]>
> Sent: Friday, November 15, 2002 10:27
> Subject: [TN] ESD Requirements in SMT Setup Area?
>
>
> >                 Hello,
> >
> > We are trying to address an issue in our SMT area where operators are
> > setting up the feeders for the machines. If they wear wrist straps while
> > sitting they have a tendency to get wrapped around everything and or
> > themselves. If we put them on their ankles, we are concerned about the
> > safety of people tripping or walking away and forgetting they are
attached
> > and doing themselves or something else harm.
> >
> > Also wondering about at the AOI station, when the operator is seated and
> > product is in the machine, as soon as they stand the 2 heel straps take
> > over. Our requirement is that as soon as you sit the wrist strap must be
> > attached. Some feel the wrist straps are not necessary for AOI.
> >
> > I am interested in how the rest of the world handles this specific ESD
> > question.  All responses are welcome, online or offline.
> >
> > Thanks,
> >
> > Carl Barnes
> > Production Process Analyst
> > 480-968-6790
> > extension: 4236
> > Page At: 602-201-1435
> >
> > ---------------------------------------------------
> > Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> > To unsubscribe, send a message to [log in to unmask] with following text
in
> > the BODY (NOT the subject field): SIGNOFF Technet
> > To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> > To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> > Search the archives of previous posts at:
http://listserv.ipc.org/archives
> > Please visit IPC web site http://www.ipc.org/html/forum.htm for
additional
> > information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> > -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
> -----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2