Hi folks
We are using combination of sulfuric acid and hydrogen peroxide as micro
etchant. We are getting black particles in the bath which sits on
conveyors and also transfered on to the panels.
We have fixed a offline filteration system for the bath from last few
weeks, the problem has come down slightly. We are cleaning all the
conveyor rods daily to avoid the black particles coming on the panels. But
this has also very less impact.
Pls suggest a way out.
thanks in advance.
Madhu
**********************************************************************
This email and any files transmitted with it are confidential and
intended solely for the use of the individual or entity to whom they
are addressed. If you have received this email in error please notify
the mail system admin at AT&S India Limited [log in to unmask]
This footnote also confirms that this email message has been swept by
MIMEsweeper for the presence of computer viruses.
www.mimesweeper.com
**********************************************************************
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------