Hi Peter,
Omega Engineering has had 1-mil-diameter T/Cs for a long time--and they are
cheaper than $140. Those thin T/Cs are not easy to work with.
Actually, the problem with T/Cs is not that they may act as heatsinks, but
actually conduct heat to the T/C junction. That is why running them through a
hole in the PCB rather than glued down to the PCB surface--typically the
hottest place for the assembly during reflow--is the better choice. The T/C
junction being in contact with the solder makes excellent contact, because it
is solder-attached.
Werner Engelmaier
Co-Chair, IPC-7530 "Guidelines for Temperature Profiling for Mass Soldering
Processes (Reflow & Wave)" Task Group
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------