TECHNET Archives

November 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-type:
text/plain; charset="us-ascii"
Sender:
Subject:
From:
"Robert J. Vega" <[log in to unmask]>
Date:
Thu, 7 Nov 2002 15:00:35 -0500
MIME-Version:
1.0
X-To:
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (128 lines)
How would you recommend placing the thermocouples and creating a profile
for a ceramic CGA?  I'm farily new at this process, and nobody here has
ever reworked a CGA.  We've been running into difficulty where the top of
our package is getting very hot before our solder joints are reaching
reflow.  Right now we have the tip of our t/c slid between columns and
placed as close to the solder joints as we could, and then taped in place.
We're using two t/c, and averaging the values.  Also, we're using a DRS-24
rework station.  According to what you say below, could we be actually be
reaching reflow, but because of the way our t/c's are placed, we're not
registering it?  If so, how could we better place them?  If not, has anyone
else had this problem?

Robert






Guy Ramsey <[log in to unmask]>@ipc.org> on 11/07/2002 01:30:08 PM

Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
       to Guy Ramsey <[log in to unmask]>

Sent by:    TechNet <[log in to unmask]>


To:    [log in to unmask]
cc:

Subject:    Re: [TN] profiling BGAs


In some packages, and with some types of reflow nozzles, your method
will not accurately reflect what is going on. In most cases it will work
fine but with a heavy board, or with a ceramic BGA, heatsinked BGA and
nozzles that heat only top of the part you may be as much as 30 degrees
off the actual temperature of the solder and pad. Your method measures
the air or board temperature between the solder balls. Which will be
stable but may not indicate when you have reached reflow.

BGA balls are brought into reflow as heat is conducted though the
package. The balls temperature (and the package temperature) can be
significantly higher than the board or air temperature under the
package. Be sure that you have not exceeded the maximum package
temperature.

Normally, we use the method you described but in difficult situations we
have drilled.
I may try Ramon's method. It sounds like it would work, unless you are
looking at .8 mm or less. When the balls are too small and the package
standoff is minimized the 3 mil wire may be a problem.

Guy Ramsey
American Competitiveness Institute
Senior Lab Technician/Instructor
Ph: (610) 362-1200 x107
Fax: (610) 362-1290



> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Tobias.Chang
> Sent: Thursday, November 07, 2002 11:25 AM
> To: [log in to unmask]
> Subject: [TN] profiling BGAs
>
>
> A couple quick questions regarding temperature profiling of
> BGA's at a re-work station.
>
> I posted maybe a month back and from the (2) responses I
> gather that drilling holes to feed the thermocouples from
> under the board is the standard practice.
>
> I tried this, however the best I could do was *attempt* to
> ensure that there was contact between the tip of the
> thermocouple and a BGA solder ball.  (the thermocouples came
> up from under the board, and I tried to place the BGA such
> the tips of the thermocouples would be in contact with the
> side of a BGA ball.  I have 3 thermocouples (middle, side,
> corner) under the BGA, and the BGA is held down by chip
> bonder at 2 opposite corners)  When I tried getting
> temperature values at the re-work station, I was getting
> inconsistent numbers.
>
> The other method I've tried was to use thermally conductive
> adhesive to hold a thermocouple between the chip and the
> board (with no drilling -> ie. the thermocouple wire lies
> flat against the board and held down by the adhesive and the
> chip).  This method seems to result in more consistent
> temperature readings.
>
> Can anyone comment on whether the adhesive method is used and
> reliable, or if theres something I'm doing wrong with the
> drilled board method?
>
> Thanks,
>
> Toby Chang
> Process Engineerin Co-op
> Leitch Technology International Inc.

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2