Jeff,
The calculation tool I have lists copper at 1.62E-08 ohm meter which is in
the same ball park you used. One interesting note is that "normal" rigid
substrates use ED copper and flex often uses RA copper as the base. Sounds
as if some confirmation is needed for the resistivity of copper in this type
of design. I agree with you regarding the other items not considered in the
calculation. Line tolerance, allowance for nicks and roughness, and the etch
factor for the circuit will affect the end result. The best etching in the
world doesn't produce a vertical side wall, and the side wall is usually a
curved or complex surface.
Just a couple more cents in the pot.
Don Vischulis
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Jeff Seeger
Sent: Thursday, November 21, 2002 1:49 PM
To: [log in to unmask]
Subject: Re: [TN] Track Resistance
> snip <
> particular tracks have to meet certain resistance.
>
> eg. Track width - 1.27mm (50 tho)
> Track Length - 68.9mm
> Copper Thickness - 105um
> Resistivity of copper 0.0000000177 ohm.metre
> Required resistance - less than 9 milli-ohms
I took the above into a PCB tool I have, and saw an expected
value of 8.67 mOhms - if everything were just perfect you make
it. A case of reality not measuring up to theory, I fear, and
will likely lead to an argument on conductivity of Cu. I lack
the time to "hit the books" but did a little with the tool and
found a startling range of answers for this question.
The default value in this tool for base copper agrees with your
value above (I'm assuming it's RA), but the value for "plated
copper foil" is only 57% of this conductivity. I did find one
anecdotal tidbit claiming ED Cu at 80% the conductivity of RA.
Here are the data points I was able to extract for your trace
at the thicknesses you've mentioned:
Case conductivity thick R
RA (base copper) 595900 mho/cm 0.075 MM 12.1389 mOhm
0.105 MM 8.67067 mOhm
0.120 MM 7.58684 mOhm
0.141 MM 6.45688 mOhm
ED (anecdotal 80%) 467720 mho/cm 0.075 MM 15.4657 mOhm
0.105 MM 11.0469 mOhm
0.120 MM 9.6660 mOhm
0.141 MM 8.2264 mOhm
"Plated" (default) 343000 mho/cm 0.075 MM 21.0892 mOhm
0.105 MM 15.0637 mOhm
0.120 MM 13.1808 mOhm
0.141 MM 11.2177 mOhm
Unfortunately this tool won't allow me to mix Cu types (as
in RA base with additive ED). I assume this would behave as
parallel resistors at DC. Also this tool makes no provision
for nicks, dish down, or other realities of life.
So it appears "Your Mileage May Vary" considerably. I'll let
you draw your own conclusions.
Good luck on this one!
--
Jeff Seeger Applied CAD Knowledge Inc
Chief Technical Officer Tyngsboro, MA 01879
jseeger "at" appliedcad "dot" com 978 649 9800
PCB Design and Implementation Services since 1983
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|