Those ramps may be too high for some packages. 4 degrees and 6 degrees
are old target values in Fahrenheit. 2 degrees is the value when using
Celsius. We have seen some parts that require ramp rates of only 1
degree C. But otherwise, no, while the recipe may vary the profile does
not.
Guy Ramsey
American Competitiveness Institute
Senior Lab Technician/Instructor
E-Mail: [log in to unmask]
Ph: (610) 362-1200 x107
Fax: (610) 362-1290
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Tobias.Chang
> Sent: Thursday, November 21, 2002 2:29 PM
> To: [log in to unmask]
> Subject: [TN] Rework vs Oven Reflow Profile
>
>
> Hello everyone,
>
> Is there any variation from the 'ideal' profile one aims for
> when developing a profile for a board in the oven, compared
> to a profile one should gun for when developing a profile for
> an individual chip when reworking a board?
>
> The 'ideal's' I'm working with are,
> max temp between 210-200 degC
> 45-75s above 183 deg C
> ramp up no more than 4 deg/s
> ramp down no more than 6 deg/s
>
> Thanks for all your help,
>
> Toby
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using
> LISTSERV 1.8e To unsubscribe, send a message to
> [log in to unmask] with following text in the BODY (NOT the
> subject field): SIGNOFF Technet To temporarily halt or
> (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE
> mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest Search the archives of
> previous posts at: http://listserv.ipc.org/archives Please
> visit IPC web site http://www.ipc.org/html/forum.htm for
> additional information, or contact Keach Sasamori at
> [log in to unmask] or 847-509-9700 ext.5315
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|