TECHNET Archives

November 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Eric Dawson <[log in to unmask]>
Date:
Tue, 19 Nov 2002 05:42:22 -0700
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, David Douthit <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=us-ascii; x-mac-type="54455854"; x-mac-creator="4D4F5353"
From:
David Douthit <[log in to unmask]>
Parts/Attachments:
text/plain (138 lines)
Erik,

Find a "hot house" garden center some where and leave them in there for a few weeks.

That should work!

David A. DOuthit
Manager
LoCan LLC

Eric Dawson wrote:

> David,
> I didn't go into too much detail because I didn't think the communication
> warranted it, but your admonition suggests I should.
> Firstly, we are a small integrated company with a Process Department of one.
> My facilities for this type of experiment are a bench (hard won through a
> bit of chicanery on my part), a Pyrex beaker (which I supplied myself) and
> access to hot water from the canteen.
> The actual conditions of soaking included total immersion in hot water,
> replenished on a daily basis, with added wetting agent. (Oh all right,
> washing up liquid) and also inverting a board with a BGA already soldered in
> place over hot water, replenished daily.
> I have also tried reflowing BGAs that have laid around the workshop for over
> a year with no moisture protection.
> And still I cannot deliberately pop corn the blighters.
> Regards
> Eric
>
> > -----Original Message-----
> > From: David Douthit [SMTP:[log in to unmask]]
> > Sent: Monday, November 18, 2002 7:31 PM
> > To:   TechNet E-Mail Forum.; Eric Dawson
> > Subject:      Re: [TN] Popcorning
> >
> > Eric,
> >
> >  Congratulations! You have proved, once again, that water vapor is much
> > more permeable than liquid water.
> >
> > Try "soaking"  them in a high humidity condition (>90%) at 40 degrees C
> > for 48 hours then running reflow.
> >
> > David A. Douthit
> > Manager
> > LoCan LLC
> >
> > Eric Dawson wrote:
> >
> > > Werner,
> > > I could use some myself for internal quality training.
> > > I have recently soaked some BGAs and some quad packs in water for over a
> > > week before putting them through a reflow profile. I have yet to produce
> > > visible evidence of pop corning.
> > > The annoying thing is, a while ago we used some BGAs on a tape where the
> > > moisture indicator went just a little pink and they pop corned. The
> > visual
> > > evidence was fat solder deposits and shorts in the middle of the package
> > > where it bowed downwards. My street cred. with the managers around here
> > has
> > > taken a beating since I have failed to reproduce the problem.
> > > Oh well, I'd rather be happy than right.
> > > Regards
> > > Eric Dawson
> > >
> > > > -----Original Message-----
> > > > From: Werner Engelmaier [SMTP:[log in to unmask]]
> > > > Sent: Monday, November 18, 2002 4:02 PM
> > > > To:   [log in to unmask]
> > > > Subject:      [TN] Popcorning
> > > >
> > > > Hi 'Netters,
> > > > Could any of share some good pictures of a 'popcorned' component and a
> > > > component with delaminated die. I would of course give full credit as
> > to
> > > > source.
> > > >
> > > > Thanks,
> > > > Werner Engelmaier
> > > >
> > > > ---------------------------------------------------
> > > > Technet Mail List provided as a free service by IPC using LISTSERV
> > 1.8e
> > > > To unsubscribe, send a message to [log in to unmask] with following text
> > in
> > > > the BODY (NOT the subject field): SIGNOFF Technet
> > > > To temporarily halt or (re-start) delivery of Technet send e-mail to
> > > > [log in to unmask]: SET Technet NOMAIL or (MAIL)
> > > > To receive ONE mailing per day of all the posts: send e-mail to
> > > > [log in to unmask]: SET Technet Digest
> > > > Search the archives of previous posts at:
> > http://listserv.ipc.org/archives
> > > > Please visit IPC web site http://www.ipc.org/html/forum.htm for
> > additional
> > > > information, or contact Keach Sasamori at [log in to unmask] or
> > 847-509-9700
> > > > ext.5315
> > > > -----------------------------------------------------
> > >
> > > ---------------------------------------------------
> > > Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> > > To unsubscribe, send a message to [log in to unmask] with following text
> > in
> > > the BODY (NOT the subject field): SIGNOFF Technet
> > > To temporarily halt or (re-start) delivery of Technet send e-mail to
> > [log in to unmask]: SET Technet NOMAIL or (MAIL)
> > > To receive ONE mailing per day of all the posts: send e-mail to
> > [log in to unmask]: SET Technet Digest
> > > Search the archives of previous posts at:
> > http://listserv.ipc.org/archives
> > > Please visit IPC web site http://www.ipc.org/html/forum.htm for
> > additional
> > > information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> > ext.5315
> > > -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> -----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2