Werner,
Interesting point you make.
But that is not at all my experience.
Is it possible that the reflowoven is an important factor for a "succesfull"
tentprofile?
Highest setting, in our reflowoven, is 250°C for extreme boards (4.4 mm)
Normally 240°C is used for boards with different types (mass) of components.
Delta T on the board is 8 - 15°C depending on the assembly.
So there is no cooking issue.
Am I overlooking something?
Jowan
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Werner Engelmaier
Sent: woensdag 13 november 2002 1:42
To: [log in to unmask]
Subject: Re: [TN] Void in BGA
Hi Daan,
I am with you on your experience. The tent-profile is really bad
news--except
for assemblies with all the same compenents, because it maximizes
temperature
differences between thermally massive components withrespect to small
components and the PWB. It also requires a different paste flux formulation,
but that is not the problem. the problem is that in order to get large
componets hot enough, the smaller ones and the PWB are cooking.
Werner Engelmaier
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
|
|
|