Phil,
I hope you are trimming prior to soldering.
The mechanical shock caused by cutters will fracture solder joints!
David A. Douthit
Manager
LoCan LLC
Phil Nutting wrote:
> Hi folks,
>
> We're still in the dark ages using through hole technology. One of the joys of TH is lead trimming and seeing just how far you can make the leads fly when you cut them.
>
> What have you other TH people done to minimize flying leads? I remember some diagonal cutters that had rubber molded into the back side to hold the leads. I also remember these were a pain in the butt. Using a high speed cutting wheel or "Q-cutter" is not an option for us due to the fact we clinch our leads and the Q-cutter just makes more work for us.
>
> Thanks in advance,
>
> Phil Nutting
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> -----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|