A 62/36/2 silver solder has a plastic state when transitioning from a solid
to a liquid of a few degrees (between 182'C to 187'C) unlike 63/37 of 183'C.
This can give enough surface tension on either side of the component to
prevent tomb stoning from occurring.
Simon.
-----Original Message-----
From: Rick Thompson [mailto:[log in to unmask]]
Sent: Wednesday, 30 October 2002 11:55 AM
To: [log in to unmask]
Subject: Re: [TN] Round Pads for 0402 Parts?
Steve,
Any feedback is appreciated. Are you saying that you've been able to
document a reduction in tombstoning on 0402's using 2% silver solder paste?
Hadn't heard of that one. Anybody else using it with these results?
Rick Thompson
===== Original Message from [log in to unmask] (TechNet E-Mail Forum.) at
10/29/02 4:37 pm
>Hi Rick!
>
>I'll get back to you tomorrow with some pad geometries that have worked
well
>here...don't trust my memory (getting senile, ya' know...hehehe)
>
>Have you tried using a 2% silver solder paste yet? I'd recommend it very
>highly!!
>Believe me, it makes a HUGE difference!!!!
>
>-Steve Gregory-
>
>---------------------------------------------------
>Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
>information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
>ext.5315
>-----------------------------------------------------
Rick Thompson
Sr. SMT Process Engineer
SMTEK International, Inc.
+1 (805) 532-2800
[log in to unmask]
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
Scanned by PeNiCillin http://safe-t-net.pnc.com.au/
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|