Thanks all, for your input. I am going to explore the defect classification
issue first.
We don't use pallets and would like to use them (and adhesives) as a last
resort. I was thinking of using a "U" shaped device that would slide onto
board and connector to clamp them together. We use board stiffeners made of
a fiberglass material that might work.
Any suggestions as to any companies who provide an off the shelf type of
camp / fixture?
Peter
-----Original Message-----
From: [log in to unmask] [mailto:[log in to unmask]]
Sent: Tuesday, October 29, 2002 4:05 PM
To: TechNet E-Mail Forum.; Crain, Peter (PS, Substation Automation
Solutions)
Subject: Re: [TN] Raised TH components after Wave
If you are running significant volumes, you might try using pallets with
topsides supports. We used them in a previous life. We had certain
connectors,
sockets, and such that "rode up" during wave and we bought some dura-stone
type
material pallets that used arms that hinged down on these pesky parts.
Jason Gregory
Production Supervisor
LaBarge Inc.
(918)459-2367
[log in to unmask]
[log in to unmask] on 10/29/2002 02:02:25 PM
Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
to
[log in to unmask]
To: [log in to unmask]
cc: (bcc: Jason Gregory/LABARGE)
Subject: [TN] Raised TH components after Wave
Hi all,
We are experiencing a large number connecters and / or sockets that are
raised after the Wave Solder process.
We classify a raised part as any gap between the PBC and the component even
though we are still keeping with IPC's standard of lead length. Is our
defect classification overkill?
If not, does anyone have this problem and can suggest a remedy?
Peter Crain
Manufacturing Engineering Technologist
Substation Automation Solutions
General Electric Canada Inc.
2728 Hopewell Place N.E., Calgary, Alberta T1Y 7J7 CANADA
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|