We are currently doing an "Acetone Test" on our incoming PWB's to test for solder mask cure.
Our test entails saturating a swab with acetone and rubbing it on the mask.

Does anyone know where this test comes from?  Is it a documented IPC test?

Also, if we do see any residue (i.e.:  green or blue discoloration on the swab), what does this
tell us and how much is enough to deem the test "failed"?

-Carrie

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2