Not sure, but I surely find this to be an IPC contradiction. Who is to say
that it was by design - maybe some operator/manufacturer short-cut their
process or forgot about it altogether?. A similar problem arises when
pre-plated leads are bent, possibly encouraging fillet problems - the place
where the main joint strength is supposed to be!
As an EMS provider, we have had fights with customers complaining about
similar situations as yours on parts they supplied, but customers tend to
think that it is always an assembly process problem.
-----Original Message-----
From: Steve Gregory [mailto:[log in to unmask]]
Sent: Thursday, October 24, 2002 4:07 PM
To: [log in to unmask]
Subject: [TN] Side and Toe Fillets...
Hi All!
I've got a situation here with a SMT socket. It's a SAMTEC CLT-105-02-L-D.
The leads are made from stamped pre-plated stock, so the sides and toes of
the leads have exposed copper, and of course doesn't wet during reflow.
In J-STD-001B, it used to say under 9.2.6.1 Flat, Ribbon, "L" and Gull Wing
Leads:
"Leads not having wettable sides or ends by design (such as leads stamped or
sheared from pre-plated stock) are not required to have side or end fillets.
In J-STD-001C it has no mention of that under the same section, in
J-STD-001C the section number has changed, it's 9.2.6.8.
So if you have leads that are made from pre-plated stock and have the sides
and toes not wet because of the exposed copper, is it now a defect? If it
is, how in the heck are you going to get the sides and toes to wet?
Thanks!
-Steve Gregory- --------------------------------------------------- Technet
Mail List provided as a free service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/html/forum.htm for additional information, or
contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
**********************************************************************
Notice:
This email transmission contains confidential information which is the property of the sender and if you are not the intended recipient, you are hereby notified that any disclosure, copying or distribution of the contents of this e-mail transmission, or the taking of any action in reliance thereon or pursuant thereto, is strictly prohibited. Should you have received this email in error, please notify us immediately to arrange for the return of the documentation comprising this transmission. No warranty is given by Tellumat (Pty) Ltd that the integrity of this e-mail has been maintained throughout transmission, nor that the communication is free of viruses, interception or interference. In no event will Tellumat (Pty) Ltd be liable to any party for any direct, indirect, special or other consequential damages for any reliance or use of this email, including, without limitation, any lost profits, business interruption, loss of programs or other data on your information handling!
system or otherwise. Unless expre
ssly stated by the sender to be given on behalf of Tellumat (Pty) Ltd, any views expressed in this message are those of the individual sender. Tellumat (Pty) Ltd disclaims liability for any unauthorised opinion or representation made by the sender on behalf of Tellumat (Pty) Ltd.
**********************************************************************
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|