Too right. The thermal degradation products include phosgene, so you
wouldn't be disappointed at all - more likely unconscious or even dead.

It's one of the prime reasons for not smoking in the presence of these non
flammable chemicals, or any others - you don't know what you'll be reacting
to form what.


Regards

Mike Fenner

Applications Engineer, European Operations
Indium Corporation
 T: + 44 1908 580 400
M: + 44 7810 526 317
 F: + 44 1908 580 411
 E: [log in to unmask]
W: www.indium.com
Leadfree: www.Pb-Free.com



-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Eric Dawson
Sent: Monday, October 21, 2002 2:59 PM
To: [log in to unmask]
Subject: Re: [TN] Flammability


And if you felt that you wanted to help the experiment along by drawing
through the lighted cigarette, within the vapours then you may be slightly
disappointed with the resultant thermal degradation products.
Regards
Eric Dawson

> -----Original Message-----
> From: Rudy Sedlak [SMTP:[log in to unmask]]
> Sent: Monday, October 21, 2002 2:35 PM
> To:   [log in to unmask]
> Subject:      Re: [TN] Flammability
>
> Doug:
>
> I have run many many flash point tests myself...
>
> The chlorinated solvents have no flash point, and will not burn at all,
> that is one of the factors that made them popular.
>
> The general rule is that the flash point is that temperature that if the
> liquid is heated to, and a cigarette thrown into it, it will burst into
> flame.  Clearly, that is a pretty low temperature for gasoline, and pretty
> high for motor oil.
>
> The chlorinated solvents will burn, but not at atmospheric pressure.
>
> Rudy Sedlak
> RD Chemical Company
> --------------------------------------------------- Technet Mail List
> provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send
> a message to [log in to unmask] with following text in the BODY (NOT the
> subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery
> of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest Search the archives of previous posts
> at: http://listserv.ipc.org/archives Please visit IPC web site
> http://www.ipc.org/html/forum.htm for additional information, or contact
> Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> -----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives