It is always a good idea to cover the cut with Solder Mask or so other
material to protect the board. Unless you really dug into the board
humidity should not effect the board.
Randy
----- Original Message -----
From: Bissonnette, Jean-Francois <[log in to unmask]>
To: <[log in to unmask]>
Sent: Wednesday, October 16, 2002 9:55 AM
Subject: [TN] conductor cut: IPC-7721
> Hi all,
>
> After cutting a trace, is it always necessary to add epoxy to fill the cut
> mark left on a board?
> If it is not filled, is there any risk of humidity infiltration that could
> cause problems latter in the
> field?
>
> Any help would be appreciated.
>
> Thanks in advance!
>
> Jean-François Bissonnette
> Vérificateur, Contrôle de la Qualité
> Électronique
> Produits et Procédés
> Vapor Rail Inc.
>
> [log in to unmask]
>
>
> WABTEC CORPORATION CONFIDENTIALITY NOTE
> The content contained in this e-mail transmission is legally privileged
and confidential information intended only for the use of the individual or
entity named herein. If the reader of this transmission is not the intended
recipient, you are hereby notified that any dissemination, distribution, or
copying of this transmission is strictly prohibited.
>
> --------------------------------------------------------------------------
-------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
> --------------------------------------------------------------------------
-------
>
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|