Susan,
Resin Coated Copper is an old product that has found a new application.
It is widely used for laser micro via drilling and most if not all the
laminators carry it. The product I know most about is Isofoil from Isola. If
you need details let me know.
Geoff Layhe
Lamar UK Ltd
One of my customers is looking for a source for RCC B stage - they report
that people used to make this and now do not - hopefully someone has a
stockpile or knows where to buy it.
Thanks for any help
Susan Mansilla
Robisan Lab
Private & Confidential:
This e-mail message is confidential and is intended solely for the person or
organisation to whom it is addressed. If the message is received by anyone
other than the addressee please return the message to the sender by replying
to it and then delete the message from your computer.
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------