Subject: | |
From: | |
Reply To: | TechNet E-Mail Forum. |
Date: | Tue, 29 Oct 2002 13:57:06 -0500 |
Content-Type: | text/plain |
Parts/Attachments: |
|
|
The process is described in J-STD-033A
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Gregg Klawson
> Sent: Tuesday, October 29, 2002 11:21 AM
> To: [log in to unmask]
> Subject: [TN] Nitrogen drying?
>
>
> Hello Technet,
>
> A question came up this morning as to whether nitrogen could
> be used as a drying agent for PWBs, components, etc. I know
> nitrogen is used as a fill gas for dry boxes, bags and to
> provide a dry atmosphere for component testing. I don't have
> a feel for the physics of using nitrogen to dry something
> out. We have a situation where baking at high temperatures
> may not be practical but immersion in a nitrogen atmosphere
> is. Any ideas, references would be appreciated.
>
> Thanks,
> Gregg
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using
> LISTSERV 1.8e To unsubscribe, send a message to
> [log in to unmask] with following text in the BODY (NOT the
> subject field): SIGNOFF Technet To temporarily halt or
> (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE
> mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest Search the archives of
> previous posts at: http://listserv.ipc.org/archives Please
> visit IPC web site http://www.ipc.org/html/forum.htm for
> additional information, or contact Keach Sasamori at
> [log in to unmask] or 847-509-9700 ext.5315
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|